1.ultra kaca bening wis akeh ngisor kaca poto bledosan rasio

Dhéfinisi bledosan dhiri: bledosan dhiri saka kaca tempered minangka fenomena pecah sing kedadeyan tanpa kekuwatan eksternal.

Titik wiwitan bledosan yaiku tengah lan nyebar kanthi radial menyang sekitar.Ing titik wiwitan bledosan diri, bakal ana rong pecahan sing relatif gedhe kanthi ciri "titik kupu".

Alasan kanggo bledosan dhewe: Jeblugan dhewe saka kaca tempered asring disebabake dening sawetara watu cilik ing lembaran kaca tempered asli.Negara kristal suhu dhuwur (a-NiS) "beku" sajrone produksi kaca lan disimpen ing suhu sekitar.Ing kaca tempered, amarga negara kristal suhu dhuwur iki ora stabil ing suhu kamar, bakal mboko sithik ngowahi menyang negara kristal suhu normal (B-NiS) kanthi wektu, lan bakal diiringi ekspansi volume tartamtu (2~ 4% ekspansi) sajrone transformasi.;Yen watu kasebut dumunung ing area tegangan tekan kaca tempered, proses transformasi fase kristal iki asring nyebabake kaca tempered pecah kanthi tiba-tiba, sing biasane diarani ledakan diri saka kaca tempered.

Tingkat bledosan saka kaca tempered sing cetha banget: Amarga kaca sing cetha banget nggunakake bahan mentah bijih kemurnian dhuwur, komposisi impurity dikurangi dadi minimal, lan komposisi NiS sing cocog uga luwih murah tinimbang kaca ngambang biasa, mula dhewe. -tingkat bledosan bisa tekan ing 2 ‱, watara 15 kaping luwih murah dibandhingake karo 3‰ tingkat bledosan dhewe saka kaca bening biasa.

warta_2_1

2. konsistensi werna

warta_2_23

Amarga isi wesi ing bahan mentah mung 1/10 utawa malah luwih murah tinimbang kaca biasa, kaca ultra-bening nyerep dawa gelombang sing kurang ijo ing cahya sing katon tinimbang kaca biasa, njamin konsistensi warna kaca.

3. kaca Ultra cetha nduweni transmitansi sing luwih dhuwur lan koefisien solar.

Parameter kaca ultra bening

kekandelan

transmisi

Refleksi

radiasi surya

koefisien shading

Ug

kedap swara

Transmisi UV

penetrating langsung

nggambarake

panyerepan

gunggung

gelombang cendhak

gelombang dawa

gunggung

(W/M2k)

Rm (dB)

Rw (dB)

2 mm

91,50%

8%

91%

8%

1%

91%

1.08

0.01

1.05

6

25

29

79%

3 mm

91,50%

8%

90%

8%

1%

91%

1.05

0.01

1.05

6

26

30

76%

3,2 mm

91,40%

8%

90%

8%

2%

91%

1.03

0.01

1.05

6

26

30

75%

4 mm

91,38%

8%

90%

8%

2%

91%

1.03

0.01

1.05

6

27

30

73%

5 mm

91,30%

8%

90%

8%

2%

90%

1.03

0.01

1.03

6

29

32

71%

6 mm

91,08%

8%

89%

8%

3%

90%

1.02

0.01

1.03

6

29

32

70%

8 mm

90,89%

8%

88%

8%

4%

89%

1.01

0.01

1.02

6

31

34

68%

10 mm

90,62%

8%

88%

8%

4%

89%

1.01

0.02

1.02

6

33

36

66%

12 mm

90,44%

8%

87%

8%

5%

88%

1.00

0.02

1.01

6

34

37

64%

15 mm

90,09%

8%

86%

8%

6%

87%

0.99

0.02

1.00

6

35

38

61%

19 mm

89,73%

8%

84%

8%

7%

86%

0.97

0.02

0.99

6

37

40

59%

4. kaca Ultra cetha nduweni transmitansi UV sing luwih murah

parameter kaca bening

kekandelan

transmisi

Refleksi

Transmisi UV

2 mm

90,80%

10%

86%

3 mm

90,50%

10%

84%

3,2 mm

89,50%

10%

84%

4 mm

89,20%

10%

82%

5 mm

89,00%

10%

80%

6 mm

88,60%

10%

78%

8 mm

88,20%

10%

75%

10 mm

87,60%

10%

72%

12 mm

87,20%

10%

70%

15 mm

86,50%

10%

68%

19 mm

85,00%

10%

66%

5. kaca ultra cetha wis kangelan produksi luwih, mangkono biaya luwih saka kaca bening

Kaca ultra bening nduweni syarat kualitas dhuwur kanggo bahan wedhi kuarsa, uga kalebu syarat dhuwur kanggo isi wesi, bijih pasir kuarsa ultra putih alami relatif langka, lan kaca ultra bening nduweni konten teknologi sing relatif dhuwur, nggawe kontrol produksi angel. iku watara 2 kaping luwih dhuwur tinimbang kaca bening.